METRIC MAHARAM_METRIC_AL
METRIC MAHARAM_METRIC_AL
-
Material TypeTextilesMaterial Sub-typeWovenPrice GradeCImage ShownDownrollBrandHaworthProgramAllianceCOM/Alliance Partner
-
Abrasion100,000FlammabilityTB117-2013Content49% POLYESTERContent51% POST IND RECYLCED POLYACT
Abrasion!
(resistance to damage from wear and rubbing)
- Heavy-duty specification ASTM 4157-02 modified (#10 cotton duck); 30,000 double rubs Wyzenbeek method.
- Heavy-duty specification ASTM D4966-98 (21 oz. weight); 40,000 cycles Martindale method.
Colorfastness to Light
(fabric retains its color when exposed to light)
All textiles meet AATCC option 1 or 3 - 2003, Class 4 minimum at 40 hours.
Physical Properties
(resistance to pilling, tearing and coming apart at the seams)
Seating upholstery meets:
- Brush pill ASTM D3511, 3-4 minimum
- Breaking strength ASTM D5034-95 50lbs. minimum in warp and weft
- Seam slippage ASTM D3597-02 D434-95 25 lbs. minimum in warp and weft.
-
CompositionWOVENWidth54 inchesWeight (Per Linear Yard)15 OZ/LYPattern Repeat HNo RepeatPattern Repeat VNo RepeatDirectionalYesBackingNo
-
Finish Code Grade Application Program AL-U22 C Seating Alliance 4X-AJ9 F Vertical COM AL-U29 C Seating Alliance 4X-DX1 F Vertical COM AL-U37 C Seating Alliance 4X-HDP F Vertical COM AL-U40 C Seating Alliance 4X-DX2 F Vertical COM AL-U44 C Seating Alliance 4X-DX4 F Vertical COM AL-U45 C Seating Alliance 4X-DX5 F Vertical COM AL-U46 C Seating Alliance 4X-KAC F Vertical COM AL-U51 C Seating Alliance 4X-DX7 F Vertical COM
-